Description

Cracks in a flexible overlay over an existing crack or joint. The cracks occur directly over the underlying cracks or joints. "Joint reflection cracking" specifically refers to reflection cracks arising from underlying PCC pavement joint movement. Reflection cracks can also occur over existing HMA pavement cracks, cement or lime stabilized base, etc.

Joint reflection cracking on an arterial.Joint reflection cracking on an arterial.Joint reflection cracking up close.
Figures 1–3. Joint reflection cracking on an arterial. Joint reflection cracking on an arterial. Joint reflection cracking up close.

Problem

Allows moisture infiltration, roughness

Possible Causes

Differential movement across the underlying crack or joint. For joint reflection cracking, this is movement of the PCC slab beneath the HMA surface because of thermal and moisture changes. Generally not load initiated, however loading can hasten deterioration.

Repair

Strategies depend upon the severity and extent of the cracking:

  • Low severity cracks (< 1/2 inch wide and infrequent cracks). Crack seal to prevent (1) entry of moisture into the subgrade through the cracks and (2) further raveling of the crack edges. In general, rigid pavement joints will eventually reflect through an HMA overlay without proper surface preparation.
  • High severity cracks (> 1/2 inch wide and numerous cracks). Remove and replace the cracked pavement layer with an overlay.

Teaching this? Figures and worked examples are free to use with credit. How to cite

Cite this page

APA

Pavement Interactive. (2018, September 24). Reflection cracking. HeadLight. Retrieved [the date you read it], from https://pavementinteractive.org/reference-desk/pavement-management/pavement-distresses/reflection-cracking/

ASCE

Pavement Interactive. (2018). “Reflection Cracking.” HeadLight, <https://pavementinteractive.org/reference-desk/pavement-management/pavement-distresses/reflection-cracking/> ([the date you read it]).

BibTeX

@misc{pavint-reflection-cracking,
  author = {{Pavement Interactive}},
  title = {Reflection Cracking},
  year = {2018},
  publisher = {HeadLight},
  howpublished = {\url{https://pavementinteractive.org/reference-desk/pavement-management/pavement-distresses/reflection-cracking/}},
  note = {Accessed [date]}
}
This address will not change. The citation records the date you read it.
Report an error

Reports go to the editors, who check them against the cited sources. Corrections are noted at the top of the article.

Only if you want a reply. It is not published.