Reinforcing steel can also be used to provide load transfer. When reinforcing steel is used, transverse contraction joints are often omitted (as in CRCP). Therefore, since there are no joints, the PCC cracks on its own and the reinforcing steel provides load transfer across these cracks. Unlike dowel bars, reinforcing steel is bonded to the PCC on either side of the crack in order to hold the crack tightly together.

Typically, rigid pavement reinforcing steel consists of grade 60 (yield stress of 60 ksi (414 MPa) No. 5 or No. 6 bars (ERES, 20011). The steel constitutes about 0.6 - 0.7 percent of the pavement cross-sectional area (ACPA, 20012) and is typically placed at slab mid-depth or shallower. At least 63 mm (2.5 inches) of PCC cover should be maintained over the reinforcing steel to minimize the potential for steel corrosion by chlorides found in deicing agents (Burke, 19833).

Teaching this? Figures and worked examples are free to use with credit. How to cite

Cite this page

APA

Pavement Interactive. (2018, September 18). Reinforcing steel. HeadLight. Retrieved [the date you read it], from https://pavementinteractive.org/reference-desk/pavement-types-and-history/pavement-types/reinforcing-steel/

ASCE

Pavement Interactive. (2018). “Reinforcing Steel.” HeadLight, <https://pavementinteractive.org/reference-desk/pavement-types-and-history/pavement-types/reinforcing-steel/> ([the date you read it]).

BibTeX

@misc{pavint-reinforcing-steel,
  author = {{Pavement Interactive}},
  title = {Reinforcing Steel},
  year = {2018},
  publisher = {HeadLight},
  howpublished = {\url{https://pavementinteractive.org/reference-desk/pavement-types-and-history/pavement-types/reinforcing-steel/}},
  note = {Accessed [date]}
}
This address will not change. The citation records the date you read it.
Sources (3)
  1. ERES (2001). Summary of CRCP Design and Construction Practices in the U.S. Concrete Reinforcing Steel Institute. Schaumburg, IL. ↩
  2. ACPA (2001). Concrete Types. Web page on the American Concrete Pavement Association's web site. Accessed 18 January 2002. ↩
  3. Burke (1983). Construction of Continuously Reinforced Concrete Pavements. Concrete Reinforcing Steel Institute. Schaumburg, IL. ↩
Report an error

Reports go to the editors, who check them against the cited sources. Corrections are noted at the top of the article.

Only if you want a reply. It is not published.