20-yr ESALs1 (millions) | Depth from Surface | |
≤ 100 mm (4 inches) | > 100 mm (4 inches) | |
< 0.3 | – | – |
0.3 to < 3 | 40 | 40 |
3 to < 10 | 45 | 40 |
10 to < 30 | 45 | 40 |
≥ 30 | 45 | 45 |
20-yr ESALs1 (millions) | Depth from Surface | |
≤ 100 mm (4 inches) | > 100 mm (4 inches) | |
< 0.3 | – | – |
0.3 to < 3 | 40 | 40 |
3 to < 10 | 45 | 40 |
10 to < 30 | 45 | 40 |
≥ 30 | 45 | 45 |