Type of Street or Highway Estimated | 18,000 lb (80 kN) ESALs |
---|---|
Parking lots, light traffic residential streets and farm roads | 5,000 |
Residential streets, rural farm and residential roads | 10,000 |
Urban and rural minor collectors | 100,000 |
Urban minor arterials, light industrial streets, rural major collectors and rural minor arterial highways | 1,000,000 |
Urban/rural freeways and other principal arterial highways | 3,000,000 |