Skip to content

Introduction to Rehabilitation

The combined effects of traffic loading and the environment will cause every pavement, no matter how well-designed/constructed to deteriorate over time. Maintenance and rehabilitation are what we use to slow down or reset this deterioration process. Maintenance actions help slow the rate of deterioration by identifying and addressing specific pavement deficiencies that contribute to overall deterioration. Rehabilitation is the act of repairing portions of an existing pavement to reset the deterioration process. Reconstructing an entire pavement, however, is not considered rehabilitation but rather new construction because the methods used are generally those developed for new pavement construction.

This section discusses common HMA and PCC pavement rehabilitation alternatives.

Rehabilitation can be defined as (ITS, 20001):

" Measures to improve, strengthen or salvage existing deficient pavements to continue service with only routine maintenance. Deficient pavements exhibit distress in excess of what can be handled through routine maintenance."

In other words, although maintenance can slow the rate of pavement deterioration, it cannot stop it. Therefore eventually the effects of deterioration need to be reversed by adding or replacing material in the existing pavement structure. This is called rehabilitation. Rehabilitation options depend upon local conditions and pavement distress types but typically include:

  • HMA overlays. Overlays are used for two primary purposes:
    • Structural overlays are designed to add structural support to the existing pavement. Because of this, they are structurally designed and are thicker than non-structural overlays.
    • Non-structural overlays are designed to add or replace the existing pavement wearing course. Because of this they contribute very little to the pavement structure and are generally assumed to provide no additional structural support. Because most agencies consider non-structural overlays to be maintenance items, they are discussed on the Maintenance page.
  • In-place recycling. There are two types of common in-place recycling:
    • Hot in-place recycling (HIPR). Covered on the recycling page.
    • Cold in-place recycling (CIPR). Covered on the recycling page. Full-depth CIPR, known as full-depth reclamation (FDR) is considered reconstruction.

Overlays are often distinguished by thickness: non-structural overlays are typically 13 to 38 mm (0.5 to 1.5 inches) thick, and structural overlays are typically thicker than 38 mm (1.5 inches). Non-structural overlays are best placed before extensive rehabilitation is needed, while cracks and potholes are still small and shallow.

Hot in-place recycling uses a specialized train of equipment and suits rural roads better than urban settings. It can correct some cracking, potholing and raveling but is not suited to heavily damaged pavements. Cold in-place recycling is meant for moderate- to low-volume roads in good structural condition with minor distresses such as shallow potholes, weathering and bleeding: the existing pavement is typically milled 50 to 100 mm (2 to 4 inches), mixed with an emulsified recycling agent, spread and compacted, and then overlaid with new HMA.

Structural Overlays

Structural overlays are used to increase pavement structural capacity. Therefore, they are considered rehabilitation, although they typically have some maintenance-type benefits as well. Asphalt concrete structural overlay design can be broadly categorized into the following (modified after Monismith and Finn, 19842):

  • Engineering judgment. This approach to overlay design selects an overlay thickness and the associated materials based on local knowledge of existing conditions, which can result in cost effective solutions; however, local expertise is fragile and subject to retirements, agency reorganizations, etc. This method is highly subjective and can be heavily influenced by political and budget constraints. Currently, more agencies appear to be relying on quantifiable overlay design approaches but tempered with local expertise.
  • Component analysis. This approach to overlay design essentially requires that the total pavement structure be developed as a new design for the specified service conditions and then compared to the existing pavement structure (taking into account pavement condition, type, and thickness of the pavement layers). Current component design procedures require substantial judgment to effectively use them. This judgment is mainly associated with selection of "weighting factors" to use in evaluating the structural adequacy of the existing pavement layers (i.e., each layer of the pavement structure is assigned a layer coefficient often on the basis of experience).
  • Non-destructive testing with limiting deflection criteria. This approach to overlay design uses pavement surface deflection measurements to determine pavement structural properties, which can then be used to determine the required amount of additional pavement structure. Basically, a pavement's surface deflection in response to a known loading is used as a measure of effective strength. This "effective strength" is influenced by a variety of factors including material properties (including subgrade), thickness of pavement layers, and environmental effects. Most currently used deflection based overlay design procedures do not attempt to isolate material properties of individual pavement layers.
  • Mechanistic-empirical analysis. This approach to overlay design uses the same mechanistic-empirical methods that were discussed in the Structural Design section. These methods are quite versatile because they can evaluate different materials under various environments and pavement conditions. In many places these procedures have replaced limiting deflection overlay methods, since the latter do not account for subsurface material properties.

Suggested Reading

  • The Asphalt Institute. (1997). Asphalt in Pavement Maintenance, Manual Series No. 16. The Asphalt Institute. Lexington, KY.
  • The Asphalt Institute. (2000). Asphalt Overlays for Highway and Street Rehabilitation, Manual Series No. 17. The Asphalt Institute. Lexington, KY.
  • Federal Highway Administration (FHWA). (June 1998). Long-Term Monitoring of Pavement Maintenance Materials Test Sites, Publication No. FHWA-RD-98-073. Office of Engineering Research and Development, Federal Highway Administration. McLean, VA.
  • National Asphalt Pavement Association (NAPA). (1995). Thin Hot Mix Asphalt Surfacings, Informational Series 110. National Asphalt Pavement Association. Lanham, MD.

Teaching this? Figures and worked examples are free to use with credit. How to cite

Cite this page

APA

Pavement Interactive. (2026, November 1). Introduction to rehabilitation. HeadLight. Retrieved [the date you read it], from https://pavementinteractive.org/reference-desk/maintenance-and-rehabilitation/rehabilitation/introduction/

ASCE

Pavement Interactive. (2026). “Introduction to Rehabilitation.” HeadLight, <https://pavementinteractive.org/reference-desk/maintenance-and-rehabilitation/rehabilitation/introduction/> ([the date you read it]).

BibTeX

@misc{pavint-introduction-to-rehabilitation,
  author = {{Pavement Interactive}},
  title = {Introduction to Rehabilitation},
  year = {2026},
  publisher = {HeadLight},
  howpublished = {\url{https://pavementinteractive.org/reference-desk/maintenance-and-rehabilitation/rehabilitation/introduction/}},
  note = {Accessed [date]}
}
This address will not change. The citation records the date you read it.
Sources (2)
  1. University of California Institute of Transportation Studies (ITS) (2000). South Africa / United States Pavement Technology Workshop, Module 3: Pavement Structural Design. Videotape series of seminar given from 20 - 23 March 2000 at the University of California Field Station. Richmond, CA. ↩
  2. Monismith, C.L. and Finn, F.N. (1984). National Cooperative Highway Research Program Synthesis of Highway Practice. 116: Asphalt Overlay Design Procedures. Transportation Research Board, National Research Council. Washington, D.C. ↩
Report an error

Reports go to the editors, who check them against the cited sources. Corrections are noted at the top of the article.