HMA structural overlays are used to increase rigid pavement structural capacity. Therefore, they are considered rehabilitation, although they typically have some maintenance-type benefits as well. Although the specific constants used may be different, flexible overlays of rigid pavement are designed in the same basic manner as flexible overlays of flexible pavement.

Teaching this? Figures and worked examples are free to use with credit. How to cite

Cite this page

APA

Pavement Interactive. (2018, August 21). Structural HMA overlays for PCC pavement. HeadLight. Retrieved [the date you read it], from https://pavementinteractive.org/reference-desk/design/structural-design/structural-hma-overlays-for-pcc-pavement/

ASCE

Pavement Interactive. (2018). “Structural HMA Overlays for PCC Pavement.” HeadLight, <https://pavementinteractive.org/reference-desk/design/structural-design/structural-hma-overlays-for-pcc-pavement/> ([the date you read it]).

BibTeX

@misc{pavint-structural-hma-overlays-for-pcc-pavement,
  author = {{Pavement Interactive}},
  title = {Structural HMA Overlays for PCC Pavement},
  year = {2018},
  publisher = {HeadLight},
  howpublished = {\url{https://pavementinteractive.org/reference-desk/design/structural-design/structural-hma-overlays-for-pcc-pavement/}},
  note = {Accessed [date]}
}
This address will not change. The citation records the date you read it.
Report an error

Reports go to the editors, who check them against the cited sources. Corrections are noted at the top of the article.

Only if you want a reply. It is not published.