Elastic modulus

The relationship between stress and strain within a material’s elastic range.

The relationship between stress and strain within a material’s elastic range. Thus, the "flexibility" of any object depends on its elastic modulus and geometric shape; however, it is important to note that strength (stress needed to break something) is not the same thing as stiffness (as measured by elastic modulus).