Sand equivalent

AASHTO T 176

Explained inSand Equivalent

Calculator

Sand equivalent

AASHTO T 176

Read to the nearest 0.1 in. (2.5 mm) from the graduated cylinder.

From the indicator on the weighted foot, less 10 in. (254 mm).

Specification

AASHTO M 323 sets 40 to 50 by traffic level.