Pavement condition index (PCI) of a sample unit

US Army TM 5-623 (PAVER)

Explained inPavement Condition Rating Systems

Calculator

Pavement condition index (PCI) of a sample unit

US Army TM 5-623 (PAVER)

One row for each distress and severity found in the sample unit. The deducts come from the PAVER curves in TM 5-623; the PCI is 100 minus their corrected total.

TM 5-623 suggests about 2,500 sq ft for asphalt.

Distresses found
RowDistressSeverityQuantity
1
2
3
4
5
6
7
8
9
10
11
12

Quantity in square feet; in feet for bumps and sags, edge cracking, joint reflection cracking, lane/shoulder drop-off and longitudinal and transverse cracking; a count for potholes. Polished aggregate has no severity.

Example values: the filled-in inspection sheets in TM 5-623 (figures 3-3 and 3-2).