Moisture content by drying (aggregate, soil, asphalt mixture)
AASHTO T 255 · T 265 · T 329Calculator
AASHTO T 255 · T 265 · T 329Moisture content by drying (aggregate, soil, asphalt mixture)
Moisture content from the wet mass and successive dry weighings, with the method’s constant-mass check.