IDEAL-CT cracking tolerance index (CTIndex)
ASTM D8225 · Tex-250-FCalculator
ASTM D8225 · Tex-250-FIDEAL-CT cracking tolerance index (CTIndex)
Enter points from the load-displacement curve, enough to follow it through the peak and down past 65 % of the peak, or the values your software reports.