Flat and elongated particles

ASTM D4791

Explained inFlat and Elongated Particles

Calculator

Flat and elongated particles

ASTM D4791
Specification

AASHTO M 323: 10 % at 5 : 1 for most traffic levels.

Example values. Your agency’s specification sets the limits.