Explained inDynamic Shear Rheometer
25 mm plate and 1 mm gap for original and RTFO binder; 8 mm plate and 2 mm gap for PAV binder.
The plate’s rotation, in degrees.
T 315 tests at 10 rad/s (1.59 Hz).