An intermediate substance in the production of portland cement. Made of heated calcium silicate, clinker is usually in the form of small gray-black pellets.

An intermediate substance in the production of portland cement. Made of heated calcium silicate, clinker is usually in the form of small gray-black pellets. Clinker is subsequently cooled and pulverized into a fine powder that almost completely passes through a 0.075 mm (No. 200) sieve and fortified with a small amount of gypsum to form portland cement.