Layer Thickness (inches) | Conversion Factor (Table 2) | Effective Thickness (inches) |
---|---|---|
75 mm (3 in.) | 0.5 | 37.5 mm (1.5 in.) |
200 mm (8 in.) | 0.2 | 40.0 mm (1.6 in.) |
Total Te equals | 77.5 mm (3.1 in.) |
Layer Thickness (inches) | Conversion Factor (Table 2) | Effective Thickness (inches) |
---|---|---|
75 mm (3 in.) | 0.5 | 37.5 mm (1.5 in.) |
200 mm (8 in.) | 0.2 | 40.0 mm (1.6 in.) |
Total Te equals | 77.5 mm (3.1 in.) |