Under 90 degrees F | Butane and lighter |
---|---|
90-220 degrees F | Gasoline |
220-315 degrees F | Naphtha |
315-450 degrees F | Kerosene |
450-800 degrees F | Gas oil |
800 degrees F and up | Residuum (including asphalt) |