# Portland Cement Loss on Ignition

Loss on ignition is calculated by heating up a cement sample to 900 - 1000°C (1650 - 1830°F) until a constant weight is obtained. The weight loss of the sample due to heating is then determined.

- Canonical URL: https://pavementinteractive.org/reference-desk/testing/cement-tests/portland-cement-loss-on-ignition/
- Last updated: 2018-06-28
- Review: reviewed by licensed professional engineers on the previous Pavement Interactive site, where reviewers were not recorded by name
- Standards: AASHTO T 105, ASTM C114

Loss on ignition is calculated by heating up a cement sample to 900 - 1000°C (1650 - 1830°F) until a constant weight is obtained. The weight loss of the sample due to heating is then determined. A high loss on ignition can indicate prehydration and carbonation, which may be caused by improper and prolonged storage or adulteration during transport or transfer (PCA, 1988[^1]).

## Standard Test Methods

- AASHTO T 105 and ASTM C 114: Chemical Analysis of [Hydraulic Cement](https://pavementinteractive.org/glossary/hydraulic-cement/)

## Sources

[^1]: Portland Cement Association (PCA) (1988). Design and Control of Concrete Mixtures. Portland Cement Association. Skokie, IL.