# PCC Pavement

Rigid pavements are so named because the pavement structure deflects very little under loading due to the high modulus of elasticity of their surface course.

- Canonical URL: https://pavementinteractive.org/reference-desk/pavement-types-and-history/pavement-types/pcc-pavement/
- Last updated: 2026-11-01

Rigid pavements are so named because the pavement structure deflects very little under loading due to the high [modulus of elasticity](https://pavementinteractive.org/reference-desk/design/design-parameters/elastic-modulus/) of their [surface course](https://pavementinteractive.org/glossary/surface-course/). A rigid pavement structure is typically composed of a PCC surface course built on top of either (1) the subgrade or (2) an underlying base course. Because of its relative rigidity, the pavement structure distributes loads over a wide area with only one, or at most two, structural layers (see Figure 1).

![Rigid Pavement Load Distribution](https://pavementinteractive.org/wp-content/uploads/2021/06/rigid_load_distribution.gif)

*Figure 1.* Rigid Pavement Load Distribution

This section describes the typical rigid pavement structure consisting of:

#### Surface course: This is the top layer, which consists of the PCC slab.

#### Base course: This is the layer directly below the PCC layer and generally consists of aggregate or stabilized subgrade.

#### Subbase course: This is the layer (or layers) under the base layer. A subbase is not always needed and therefore may often be omitted.

## Structural Elements

A typical rigid pavement structure (see Figure 2) consists of the surface course and the underlying base and subbase courses (if used). The surface course (made of PCC) is the stiffest (as measured by [resilient modulus](https://pavementinteractive.org/reference-desk/design/design-parameters/resilient-modulus/)) and provides the majority of strength. The underlying layers are orders of magnitude less stiff but still make important contributions to pavement strength as well as drainage and frost protection.

![Basic rigid pavement structure](https://pavementinteractive.org/wp-content/uploads/2021/06/rigid-pavement.jpg)

*Figure 2.* Basic rigid pavement structure.

### Surface Course

The surface course is the layer in contact with traffic loads and is made of PCC. It provides characteristics such as [friction](https://pavementinteractive.org/reference-desk/pavement-management/pavement-evaluation/skid-resistance/) (see Figure 3), [smoothness](https://pavementinteractive.org/reference-desk/pavement-management/pavement-evaluation/roughness/), noise control and drainage. In addition, it serves as a waterproofing layer to the underlying base, subbase and subgrade. The surface course can vary in thickness but is usually between 150 mm (6 inches) (for light loading) and 300 mm (12 inches) (for heavy loads and high traffic). Figure 4 shows a 300 mm (12 inch) surface course.

![PCC Surface](https://pavementinteractive.org/wp-content/uploads/2009/06/Pcc2.jpg)

![Rigid Pavement Slab Thickness](https://pavementinteractive.org/wp-content/uploads/2009/06/Pcc_thickness1.jpg)

*Figures 3 and 4.* PCC Surface Rigid Pavement Slab Thickness

### Base Course

The base course is immediately beneath the surface course. It provides (1) additional load distribution, (2) contributes to drainage and frost resistance, (3) uniform support to the pavement and (4) a stable platform for construction equipment (ACPA, 2001). Bases also help prevent subgrade soil movement due to slab pumping. Base courses are usually constructed out of:

1. *Aggregate base*. A simple base course of crushed aggregate has been a common option since the early 1900s and is still appropriate in many situations today.
2. *Stabilized aggregate or soil (see Figure 5)*. Stabilizing agents are used to bind otherwise loose particles to one another, providing strength and cohesion. Cement treated bases (CTBs) can be built to as much as 20 - 25 percent of the surface course strength (FHWA, 1999). However, cement treated bases (CTBs) used in the 1950s and early 1960s had a tendency to lose excessive amounts of material leading to panel cracking and settling.
3. *Dense-graded HMA*. In situations where high base stiffness is desired base courses can be constructed using a dense-graded HMA layer.
4. *[Permeable HMA](https://pavementinteractive.org/reference-desk/pavement-types-and-history/pavement-types/permeable-pavements/)*. In certain situations where high base stiffness and excellent drainage is desired, base courses can be constructed using an open graded HMA. Recent research may indicate some significant problems with ATPB use.
5. *Lean concrete (see Figure 6)*. Contains less [portland cement](https://pavementinteractive.org/glossary/portland-cement/) paste than a typical PCC and is stronger than a stabilized aggregate. Lean concrete bases (LCBs) can be built to as much as 25 - 50 percent of the surface course strength (FHWA, 1999). A lean concrete base functions much like a regular PCC surface course and therefore, it requires [construction joints](https://pavementinteractive.org/reference-desk/construction/placement/joints/) and will crack over time. These joints and cracks can potentially cause [reflection cracking](https://pavementinteractive.org/glossary/reflection-cracking/) in the surface course if they are not carefully matched.

![Completed CTB with Curing Seal](https://pavementinteractive.org/wp-content/uploads/2009/06/Ctb.jpg)

![Lean Concrete Base Material](https://pavementinteractive.org/wp-content/uploads/2009/06/Lean_concrete.jpg)

*Figures 5 and 6.* Completed CTB with Curing Seal Lean Concrete Base Material

### Subbase Course

The subbase course is the portion of the pavement structure between the base course and the subgrade. It functions primarily as structural support but it can also:

1. Minimize the intrusion of fines from the subgrade into the pavement structure.
2. Improve drainage.
3. Minimize [frost action damage](https://pavementinteractive.org/reference-desk/design/design-parameters/frost-action/).
4. Provide a working platform for construction.

The subbase generally consists of lower quality materials than the base course but better than the subgrade soils. Appropriate materials are aggregate and high quality structural fill. A subbase course is not always needed or used.

## Types

Almost all rigid pavement is made with Portland Cement Concrete (PCC). Rigid pavements are differentiated into three major categories by their means of crack control:

**#### [Jointed plain concrete pavement (JPCP)](https://pavementinteractive.org/reference-desk/pavement-types-and-history/pavement-types/jointed-plain-concrete-pavement/)**

This is the most common type of rigid pavement. JPCP controls cracks by dividing the pavement up into individual slabs separated by [contraction joints](https://pavementinteractive.org/glossary/contraction-joint/). Slabs are typically one lane wide and between 3.7 m (12 ft.) and 6.1 m (20 ft.) long. JPCP does not use any reinforcing steel but does use dowel bars and tie bars.

**#### [Jointed reinforced concrete pavement (JRCP)](https://pavementinteractive.org/reference-desk/pavement-types-and-history/pavement-types/jointed-reinforced-concrete-pavement/)**

As with JPCP, JRCP controls cracks by dividing the pavement up into individual slabs separated by contraction joints. However, these slabs are much longer (as long as 15 m (50 ft.)) than JPCP slabs, so JRCP uses reinforcing steel within each slab to control within-slab cracking. This pavement type is no longer constructed in the U.S. due to some long-term performance problems.

**#### [Continuously reinforced concrete pavement (CRCP)](https://pavementinteractive.org/reference-desk/pavement-types-and-history/pavement-types/continuously-reinforced-concrete-pavement/)**

This type of rigid pavement uses reinforcing steel rather than contraction joints for crack control. Cracks typically appear ever 1.1 - 2.4 m (3.5 - 8 ft.) are held tightly together by the underlying reinforcing steel. [FHWA Tech Brief.](https://www.fhwa.dot.gov/pavement/concrete/pubs/hif12039/hif12039.pdf)

## Durability

A durable PCC pavement resists the environmental forces that would otherwise cause premature deterioration. Durability has traditionally been associated with high cement content, which lowers the water-cement ratio and the permeability of the concrete, and lower permeability does correlate well with durability. But durability is a general quality rather than a single property: [strength](https://pavementinteractive.org/reference-desk/testing/cement-tests/compressive-strength/), water-cement ratio and air voids all contribute, none of them alone predicts how durable a pavement will be, and the mix must be designed for the particular environment. The main concerns are:

- **Freezing and thawing.** Water expands when it freezes, so the paste needs a system of small, uniformly distributed air voids into which it can expand. Air trapped during mixing and voids left by evaporating water are haphazard and usually inadequate, so air is deliberately entrained through [admixtures](https://pavementinteractive.org/reference-desk/design/mix-design/pcc-admixtures/) and adjustments to [mix design](https://pavementinteractive.org/reference-desk/design/mix-design/pcc-mix-design-fundamentals/), production and [placement](https://pavementinteractive.org/reference-desk/construction/placement/pcc-placement/). Concrete with an adequate air-void system that has cured to sufficient strength should resist [freeze-thaw damage](https://pavementinteractive.org/glossary/freeze-thaw-damage/).
- **Reactive aggregates.** Because cement is highly alkaline, some aggregates react with it; aggregates containing highly reactive silica can cause severe cracking through [alkali-silica reaction](https://pavementinteractive.org/reference-desk/pavement-management/pavement-distresses/alkali-aggregate-reaction/). The remedy is nonreactive aggregate or, where none is available, supplementary materials that mitigate the reaction. Aggregate [durability and soundness](https://pavementinteractive.org/reference-desk/materials/aggregate/durability-and-soundness/) matter as well.
- **Chemical attack.** Where sulfates in soil or water, or deicing chemicals, are a concern, a lower water-cement ratio reduces permeability and so slows penetration, and particular cement types and supplementary materials can improve resistance.
- **Construction.** Proper [consolidation](https://pavementinteractive.org/reference-desk/construction/placement/pcc-consolidation/) gives a uniform mix and air-void system, and proper [finishing](https://pavementinteractive.org/reference-desk/construction/placement/pcc-finishing/) and [curing](https://pavementinteractive.org/reference-desk/construction/placement/pcc-curing/) give the concrete the conditions it needs to develop strength, abrasion resistance and low permeability during hydration.

See [PCC Durability](https://pavementinteractive.org/reference-desk/materials/portland-cement/pcc-durability/) for more.