# Load Transfer

"Load transfer" is a term used to describe the transfer (or distribution) load across discontinuities such as joints or cracks (AASHTO, 1993).

- Canonical URL: https://pavementinteractive.org/reference-desk/pavement-types-and-history/pavement-types/load-transfer/
- Last updated: 2026-11-01
- Review: reviewed by licensed professional engineers on the previous Pavement Interactive site, where reviewers were not recorded by name

"Load transfer" is a term used to describe the transfer (or distribution) load across discontinuities such as joints or cracks (AASHTO, 1993[^1]). When a wheel load is applied at a joint or crack, both the loaded slab and adjacent unloaded slab deflect. The amount the unloaded slab deflects is directly related to joint performance. If a joint is performing perfectly, both the loaded and unloaded slabs deflect equally. Load transfer efficiency is defined by the following equation:

$$\text{Efficiency}\ (\%) = \frac{\Delta_a}{\Delta_l} \times 100$$

where:

- $$\Delta_a$$ = approach slab deflection
- $$\Delta_l$$ = leave slab deflection

This efficiency depends on several factors, including temperature (which affects joint opening), joint spacing, number and magnitude of load applications, foundation support, aggregate particle angularity, and the presence of mechanical load transfer devices. Figure 1 illustrates the extremes in load transfer efficiency. Most performance problems with concrete pavement are a result of poorly performing joints (ACPA, 2001). Poor load transfer creates high slab stresses, which contribute heavily to distresses such as [faulting](https://pavementinteractive.org/reference-desk/pavement-management/pavement-distresses/faulting/), [pumping](https://pavementinteractive.org/reference-desk/pavement-management/pavement-distresses/pumping/) and [corner breaks](https://pavementinteractive.org/reference-desk/pavement-management/pavement-distresses/corner-break/). Thus, adequate load transfer is vital to [rigid pavement](https://pavementinteractive.org/glossary/rigid-pavement/) performance.

## Methods

Load transfer across transverse joints/cracks is generally accomplished using one of the following:

- [Aggregate Interlock](https://pavementinteractive.org/glossary/aggregate-interlock/)
- [Dowel Bars](https://pavementinteractive.org/glossary/dowel-bar/)
- Reinforcing Steel

[Watch the video](https://pavementinteractive.org/wp-content/uploads/2021/06/load_transfer.mp4)

Figure 1. Load Transfer Efficiency Across a PCC [Surface Course](https://pavementinteractive.org/glossary/surface-course/) Joint

## Sources

[^1]: AASHTO (1993). AASHTO Guide for Design of Pavement Structures. American Association of State Highway and Transportation Officials. Washington, D.C.