# Raveling

The progressive disintegration of an HMA layer from the surface downward as a result of the dislodgement of aggregate particles.

- Canonical URL: https://pavementinteractive.org/reference-desk/pavement-management/pavement-distresses/raveling/
- Last updated: 2018-09-21
- Review: reviewed by licensed professional engineers on the previous Pavement Interactive site, where reviewers were not recorded by name

## Description

The progressive disintegration of an HMA layer from the surface downward as a result of the dislodgement of aggregate particles.

![Raveling due to low density.](https://pavementinteractive.org/wp-content/uploads/2009/04/WSDOT151.jpg)

![Raveling from snowplow operations.](https://pavementinteractive.org/wp-content/uploads/2009/04/WSDOT152.jpg)

![Raveling caused by segregation.](https://pavementinteractive.org/wp-content/uploads/2009/04/WSDOT129.jpg)

*Figures 1–3.* Raveling due to low density. Raveling from snowplow operations. Raveling caused by segregation.

## Problem

Loose debris on the pavement, [roughness](https://pavementinteractive.org/reference-desk/pavement-management/pavement-evaluation/roughness/), water collecting in the raveled locations resulting in vehicle hydroplaning, loss of [skid resistance](https://pavementinteractive.org/reference-desk/pavement-management/pavement-evaluation/skid-resistance/)

## Possible Causes

Several including:

- Loss of bond between aggregate particles and the [asphalt binder](https://pavementinteractive.org/glossary/asphalt-binder/) as a result of:

  - A dust coating on the aggregate particles that forces the asphalt binder to bond with the dust rather than the aggregate
  - [Aggregate Segregation](https://pavementinteractive.org/reference-desk/construction/placement/aggregate-segregation/). If fine particles are missing from the aggregate matrix, then the asphalt binder is only able to bind the remaining coarse particles at their relatively few contact points.
  - [Inadequate compaction during construction](https://pavementinteractive.org/reference-desk/construction/compaction/hma-compaction/). High density is required to develop sufficient cohesion within the HMA. The third figure above shows a road suffering from raveling due to inadequate compaction caused by [cold weather paving](https://pavementinteractive.org/reference-desk/construction/compaction/cold-weather-paving/).

- Mechanical dislodging by certain types of traffic ([studded tires](https://pavementinteractive.org/reference-desk/design/design-parameters/studded-tire-information/), snowplow blades or tracked vehicles). The first and fourth figures above show raveling most likely caused by snow plows.

## Repair

A raveled pavement should be investigated to determine the root cause of failure. Repair strategies generally fall into one of two categories:

- **Small, localized areas of raveling**. Remove the raveled pavement and [patch](https://pavementinteractive.org/reference-desk/maintenance-and-rehabilitation/maintenance/hma-patching/).
- **Large raveled areas indicative of general HMA failure**. Remove the damaged pavement and [overlay](https://pavementinteractive.org/reference-desk/maintenance-and-rehabilitation/rehabilitation/overlay/).