# Foamed Asphalt

Foamed asphalt is formed by combining hot asphalt binder with small amounts of cold water.

- Canonical URL: https://pavementinteractive.org/reference-desk/materials/asphalt/foamed-asphalt/
- Last updated: 2018-09-18
- Review: reviewed by licensed professional engineers on the previous Pavement Interactive site, where reviewers were not recorded by name

Foamed asphalt is formed by combining hot [asphalt](https://pavementinteractive.org/reference-desk/materials/asphalt/introduction/) binder with small amounts of cold water. When the cold water comes in contact with the hot [asphalt binder](https://pavementinteractive.org/glossary/asphalt-binder/) it turns to steam, which becomes trapped in tiny asphalt binder bubbles (World Highways, 2001[^1]). The result is a thin-film, high volume asphalt foam with approximately 10 times more coating potential than the asphalt binder in its normal liquid state (World Highways, 2001[^1]). This high volume foam state only lasts for a few minutes, after which the asphalt binder resumes its original properties. Foamed asphalt can be used as a binder in soil or [base course](https://pavementinteractive.org/glossary/base-course/) stabilization, and is often used as the stabilizing agent in [full-depth asphalt](https://pavementinteractive.org/glossary/full-depth-asphalt/) reclamation.

## Sources

[^1]: World Highways (2001). Foamed Asphalt Takes Hold. World Highways, April 2001.