# Cutback Asphalt

A cutback asphalt is simply a combination of asphalt cement and petroleum solvent.

- Canonical URL: https://pavementinteractive.org/reference-desk/materials/asphalt/cutback-asphalt/
- Last updated: 2018-09-18
- Review: reviewed by licensed professional engineers on the previous Pavement Interactive site, where reviewers were not recorded by name

A cutback asphalt is simply a combination of [asphalt cement](https://pavementinteractive.org/glossary/asphalt-cement/) and petroleum solvent. Like [emulsions](https://pavementinteractive.org/reference-desk/materials/asphalt/emulsified-asphalt/), cutbacks are used because they reduce asphalt viscosity for lower temperature uses ([tack coats](https://pavementinteractive.org/reference-desk/construction/site-preparation/tack-coats/), [fog seals](https://pavementinteractive.org/reference-desk/maintenance-and-rehabilitation/maintenance/fog-seals/), [slurry seals](https://pavementinteractive.org/reference-desk/maintenance-and-rehabilitation/maintenance/slurry-seals/), stabilization material). Similar to emulsified asphalts, after a cutback asphalt is applied the petroleum solvent evaporates leaving behind asphalt cement residue on the surface to which it was applied. A cutback asphalt is said to "cure" as the petroleum solvent evaporates away. The use of cutback asphalts is decreasing because of (Roberts et al., 1996[^1]):

- **Environmental regulations**. Cutback asphalts contain volatile chemicals that evaporate into the atmosphere. Emulsified asphalts evaporate water into the atmosphere.
- **Loss of high energy products**. The petroleum solvents used require higher amounts of energy to manufacture and are expensive compared to the water and [emulsifying agents](https://pavementinteractive.org/glossary/emulsifying-agent/) used in emulsified asphalts.

In many places, cutback asphalt use is restricted to patching materials for use in cold weather.

## Sources

[^1]: Roberts, F.L.; Kandhal, P.S.; Brown, E.R.; Lee, D.Y. and Kennedy, T.W. (1996). Hot Mix Asphalt Materials, Mixture Design, and Construction. National Asphalt Pavement Association Education Foundation. Lanham, MD.