# Asphalt Specific Gravity

Because the specific gravity of asphalt binders change with temperature, specific gravity tests are useful in making volume corrections based on temperature.

- Canonical URL: https://pavementinteractive.org/reference-desk/materials/asphalt/asphalt-specific-gravity/
- Last updated: 2017-04-27
- Review: reviewed by licensed professional engineers on the previous Pavement Interactive site, where reviewers were not recorded by name
- Standards: AASHTO T 228, ASTM D70, AASHTO M 132

Because the specific gravity of [asphalt binders](https://pavementinteractive.org/glossary/asphalt-binder/) change with temperature, specific gravity tests are useful in making volume corrections based on temperature. The specific gravity at 15.6° C (60° F) is commonly used when buying/selling [asphalt cements](https://pavementinteractive.org/glossary/asphalt-cement/). A typical specific gravity for asphalt is around 1.03.

## Related Tests

- AASHTO T 228 and ASTM D 70: Specific Gravity and Density of Semi-Solid Bituminous Materials