# Overlay

An overlay is any operation that consists of laying either Portland Cement Concrete (PCC) or Hot Mix Asphalt (HMA) over an existing pavement structure.

- Canonical URL: https://pavementinteractive.org/reference-desk/maintenance-and-rehabilitation/rehabilitation/overlay/
- Last updated: 2018-07-30
- Review: reviewed by licensed professional engineers on the previous Pavement Interactive site, where reviewers were not recorded by name

An overlay is any operation that consists of laying either [Portland Cement](https://pavementinteractive.org/glossary/portland-cement/) Concrete (PCC) or [Hot Mix Asphalt](https://pavementinteractive.org/glossary/hot-mix-asphalt-hma/) (HMA) over an existing pavement [structure](https://pavementinteractive.org/reference-desk/design/structural-design/pavement-structure/). This is different than a total replacement of the structure, and is typically done when there is only minor to modest damage to the existing pavement structure.

When constructing an overlay, the old surface is typically [milled](https://pavementinteractive.org/reference-desk/construction/site-preparation/existing-surface-preparation-for-overlays/) or ground off. Any minor structural deficiencies are then repaired. Finally, a new surface is applied.