# Structural Number

The Structural Number (SN) represents the overall structural requirement needed to sustain the design's traffic loadings.

- Canonical URL: https://pavementinteractive.org/reference-desk/design/structural-design/structural-number/
- Last updated: 2026-11-01

The Structural Number (SN) represents the overall structural requirement needed to sustain the design's traffic loadings. It is an abstract number that expresses the structural strength of a pavement required for given combinations of soil support ($$M_{R}$$), total traffic expressed in ESALs, terminal serviceability and environment.

The following equation can be used to relate individual material types and thicknesses to the structural number:

SN = a₁D₁ + a₂D₂M₂ + a₃D₃M₃

where:

- a₁, a₂, a₃ = structural-layer coefficients of the wearing surface, base, and subbase layers, respectively,
- D₁, D₂, D₃ = thickness of the wearing surface, base, and subbase layers in inches, respectively, and
- M₂, M₃ = drainage coefficients for the base and subbase, respectively.

The Structural Number is converted to actual layer thicknesses (e.g., 150 mm (6 inches) of HMA) using a layer coefficient (a) that represents the relative strength of the construction materials in that layer. Additionally, all layers below the [surface layer](https://pavementinteractive.org/glossary/surface-layer/) are assigned a drainage coefficient (m) that represents the relative loss of strength in a layer due to its drainage characteristics and the total time it is exposed to near-saturation moisture conditions. The drainage coefficient is often assumed to be 1, although quick-draining layers that almost never become saturated can have coefficients as high as 1.4 while slow-draining layers that are often saturated can have drainage coefficients as low as 0.40. Keep in mind that a drainage coefficient is basically a way of making a specific layer thicker, but not necessarily more dense. If a fundamental drainage problem is suspected, a better solution is to address the actual drainage problem by using very dense layers (to minimize water infiltration) or designing a drainage system.

## Determining the Structural Number and Layer Thicknesses

In the [1993 AASHTO flexible pavement design procedure](https://pavementinteractive.org/reference-desk/design/structural-design/1993-aashto-flexible-pavement-structural-design/), the design equation is most commonly solved for the required SN, given the design traffic, subgrade [resilient modulus](https://pavementinteractive.org/glossary/resilient-modulus/), serviceability loss and reliability. The layer equation above is then used to choose thicknesses that supply that SN. It can be extended to any number of layers, with subscripts numbered from the top of the structure down.

Layer coefficients are usually determined empirically from the performance of the material, and agencies often set values for commonly used materials as design policy. Some typical values are:

| Material | Layer coefficient (a) |
|---|---|
| Hot mix asphalt | 0.44 |
| Road mix (low stability) | 0.20 |
| Aggregate base | 0.13 |
| Engineered fill | 0.10 |

Because the coefficient depends on the material's properties and on its position in the structure, other values may be appropriate for local conditions.

With more than one structural layer, many combinations of thicknesses can give the required SN. The relative costs of the materials and practical construction limits, such as avoiding layers that are excessively thick or thin, usually narrow the choice to a particular combination.

The same relationship can be used to evaluate an existing pavement. Entering the existing layer thicknesses and coefficients gives the SN of the pavement in place; comparing it with the SN required for the new design traffic indicates the type and thickness of rehabilitation needed.

Calculator: Structural number from layers — https://pavementinteractive.org/tools/structural-number/