# Mechanistic-Empirical Pavement Design

Mechanics is the science of motion and the action of forces on bodies. Thus, a mechanistic approach seeks to explain phenomena only by reference to physical causes.

- Canonical URL: https://pavementinteractive.org/reference-desk/design/structural-design/mechanistic-empirical-pavement-design/
- Last updated: 2026-11-01

Mechanics is the science of motion and the action of forces on bodies. Thus, a mechanistic approach seeks to explain phenomena only by reference to physical causes. In pavement design, the phenomena are the stresses, strains and deflections within a pavement structure, and the physical causes are the loads and material properties of the pavement structure. The relationship between these phenomena and their physical causes is typically described using a mathematical model. Various mathematical models can be (and are) used; the most common is a layered elastic model.

Along with this mechanistic approach, empirical elements are used when defining what value of the calculated stresses, strains and deflections result in pavement failure. The relationship between physical phenomena and pavement failure is described by empirically derived equations that compute the number of loading cycles to failure.

The basic advantages of a mechanistic-empirical pavement design method over a [purely empirical one](https://pavementinteractive.org/reference-desk/design/structural-design/empirical-pavement-design/) are:

- It can be used for both [existing pavement rehabilitation](https://pavementinteractive.org/reference-desk/maintenance-and-rehabilitation/rehabilitation/introduction/) and new pavement construction
- It accommodates changing load types
- It can better characterize materials allowing for:

  - Better utilization of available materials
  - Accommodation of new materials
  - An improved definition of existing layer properties

- It uses material properties that relate better to actual pavement performance
- It provides more reliable performance predictions
- It better defines the role of construction
- It accommodates environmental and aging effects on materials

The benefit of a mechanistic-empirical approach is its ability to accurately characterize in situ material (including [subgrade](https://pavementinteractive.org/reference-desk/design/design-parameters/subgrade/) and existing pavement structures). This is typically done by using a portable device (like a [FWD](https://pavementinteractive.org/reference-desk/pavement-management/pavement-evaluation/deflection/)) to make actual field [deflection measurements](https://pavementinteractive.org/reference-desk/pavement-management/pavement-evaluation/deflection/) on a pavement structure to be overlaid. These measurements can then be input into equations to determine existing pavement structural support (often called "[backcalculation](https://pavementinteractive.org/glossary/backcalculation/)") and the approximate remaining pavement life. This allows for a more realistic design for the given conditions.

## The Mechanistic-Empirical Pavement Design Guide (MEPDG)

The Mechanistic-Empirical Pavement Design Guide (MEPDG), developed with accompanying software under NCHRP Project 1-37A, applies this approach to the design of new and rehabilitated pavements. It was intended to update the 1993 AASHTO *Guide for Design of Pavement Structures*, which is based largely on empirical observations from the AASHO Road Test of the 1950s. The MEPDG's performance models are calibrated with data from the Long-Term Pavement Performance (LTPP) program, which covers a far wider range of designs and traffic than the Road Test.

### Design Process

Conventional empirical methods take the inputs and produce a required pavement structure. The MEPDG works the other way. A trial pavement structure is assumed along with traffic and climate inputs, and the software computes how the structure responds to loading and environmental stresses and how damage accumulates over time, expressed as predicted [distresses](https://pavementinteractive.org/reference-desk/pavement-management/pavement-distresses/general-guidance-2/) and loss of [ride quality](https://pavementinteractive.org/glossary/ride-quality/). The designer then asks two questions:

1. Does the predicted performance satisfy the design criteria, such as the desired service life, given the predicted distress and maintenance and rehabilitation needs? The owning agency typically specifies the criteria, or the designer judges whether the predicted performance is acceptable.
2. Are there reasonable alternatives to the trial assumptions that would give better predicted performance or lower [life-cycle cost](https://pavementinteractive.org/reference-desk/pavement-management/analysis/life-cycle-cost-analysis/)?

The second question is asked even when the trial design is acceptable, because the method is iterative: trying variations shows which factors matter most for the project and gives more confidence that the selected design is the best one for the conditions. Where designers had been using overly conservative assumptions, mechanistic-empirical analysis has in some cases indicated that initial construction costs could be reduced.

### Performance Indicators

The MEPDG predicts [roughness](https://pavementinteractive.org/reference-desk/pavement-management/pavement-evaluation/roughness/), as the [International Roughness Index](https://pavementinteractive.org/glossary/international-roughness-index-iri/) (IRI), for all pavement types, plus indicators specific to each type:

- **Asphalt pavements:** [rutting](https://pavementinteractive.org/reference-desk/pavement-management/pavement-distresses/rutting/), [fatigue (alligator) cracking](https://pavementinteractive.org/reference-desk/pavement-management/pavement-distresses/fatigue-cracking/), [longitudinal cracking](https://pavementinteractive.org/reference-desk/pavement-management/pavement-distresses/longitudinal-cracking/) and [transverse cracking](https://pavementinteractive.org/reference-desk/pavement-management/pavement-distresses/transverse-cracking/).
- **[Jointed plain concrete pavement (JPCP)](https://pavementinteractive.org/reference-desk/pavement-types-and-history/pavement-types/jointed-plain-concrete-pavement/):** joint [faulting](https://pavementinteractive.org/reference-desk/pavement-management/pavement-distresses/faulting/) and slab cracking.
- **[Continuously reinforced concrete pavement (CRCP)](https://pavementinteractive.org/reference-desk/pavement-types-and-history/pavement-types/continuously-reinforced-concrete-pavement/):** [punchouts](https://pavementinteractive.org/reference-desk/pavement-management/pavement-distresses/punchout/).

### Input Hierarchy

The MEPDG relies on detailed material and traffic inputs, which can take extensive testing and data collection to obtain. Inputs are therefore entered hierarchically: the user supplies whatever level of detail is available and the software adjusts. Traffic is an example. At the lowest level, only an estimate of traffic volume is given, and the software assumes a typical distribution of vehicle types to derive [loads](https://pavementinteractive.org/reference-desk/design/design-parameters/loads/). With site traffic counts that include vehicle class, a higher input level is possible, although the load spectrum for each class must still be assumed. At the highest level, weigh-in-motion data near the site give the actual load distribution as well as volumes. Higher levels increase the precision of the design, but the procedure still works at lower levels.

The software also draws on built-in data: its performance models come primarily from the LTPP database, and, as originally released, it included climate data from more than 800 weather stations so that a design could use the stations nearest the project.