# Batch Plant & Mix Design

The asphalt originated from Lakeside Industries' drum plant (see Figure 1) in Issaquah, WA which is approximately 20 miles from the project site. This counter flow drum plant uses natural gas or diesel fuel to dry/heat the aggregate.

- Canonical URL: https://pavementinteractive.org/reference-desk/design/mix-design/batch-plant-mix-design/
- Last updated: 2026-11-01
- Review: reviewed by licensed professional engineers on the previous Pavement Interactive site, where reviewers were not recorded by name

## Batch Plant

The asphalt originated from [Lakeside Industries'](http://www.lakesideind.com) [drum plant](https://pavementinteractive.org/glossary/drum-plant/) (see Figure 1) in [Issaquah, WA](http://www.google.com/maps?q=Issaquah,+WA,+USA&sa=X&oi=map&ct=title|) which is approximately 20 miles from the project site. This counter flow [drum plant](https://pavementinteractive.org/reference-desk/construction/production/hma-drum-plant/) uses natural gas *or* diesel fuel to dry/heat the aggregate. The fuel source can be changed as necessary to use the least expensive fuel available. The output of this plant is 500 tons/hour, but can be increased slightly to full capacity, as operations require. The HMA is stored in one of four [storage silos](https://pavementinteractive.org/reference-desk/construction/transportation/hma-transport/) (see Figure 2) until it is placed in [trucks](https://pavementinteractive.org/reference-desk/construction/transportation/end-dump-truck/) and transported to the site. The system is fully automated to produce the exact mix design required in the project specifications.

[Lakeside](http://www.lakesideind.com/) owns the entire aggregate pit where the drum plant resides, but it shares the site with [Cadman Heidelburg Cement Group](http://www.cadman.com/) who operates a [concrete batch plant](https://pavementinteractive.org/reference-desk/construction/production/central-mixed-pcc/) on the site. The site houses a pit, aggregate crushers, sorting equipment, aggregate stockpiles, a concrete batch plant, a [HMA drum plant](https://pavementinteractive.org/reference-desk/construction/production/hma-drum-plant/), equipment maintenance space, QC testing facilities, and all the support equipment one might expect for this operation. Both Lakeside and Cadman have large stockpiles (see Figure 3) of aggregate and Recycled Hot Mix on the site for their daily plant operations.

![Lakeside Industries HMA Drum Plant, Issaquah WA](https://pavementinteractive.org/wp-content/uploads/2008/04/Lakeside_Drum_Plant.jpg)

*Figure 1.* Lakeside Industries HMA Drum Plant, Issaquah WA

![HMA storage silos at Lakeside Industries drum plant](https://pavementinteractive.org/wp-content/uploads/2008/04/Lakeside_Ind_silos.jpg)

![Stockpiles and pit at Lakeside Industries drum plant](https://pavementinteractive.org/wp-content/uploads/2008/04/Lakeside_Ind_pit_and_stockpiles.jpg)

*Figures 2 and 3.* HMA storage silos at Lakeside Industries drum plant Stockpiles and pit at Lakeside Industries drum plant

## Mix Design

The contractor submitted a mix design and samples to SDOT, which in turn used WSDOT testing laboratories for validation of the contractor's test results. The validation process approved the mix design for use on this project (see [Lakeside Verification Report](https://pavementinteractive.org/wp-content/uploads/2008/04/Lakeside_Verification_Report1.pdf)).

A higher grade HMA, PG 70-22, was used on this job because traffic consists of both *very slow-moving* vehicles and a *high* proportion of buses. This higher grade HMA mix should better resist [rutting](https://pavementinteractive.org/glossary/rutting/) and [shoving](https://pavementinteractive.org/glossary/shoving/). Of interesting note, the project specification disallows the use of Recycled Asphalt Pavement (RAP) with PG 70-22.