# Loads

One of the primary functions of a pavement is load distribution. Therefore, in order to adequately design a pavement something must be known about the expected loads it will encounter.

- Canonical URL: https://pavementinteractive.org/reference-desk/design/design-parameters/loads/
- Last updated: 2026-11-01

One of the primary functions of a pavement is load distribution. Therefore, in order to adequately design a pavement something must be known about the expected loads it will encounter. Loads, the vehicle forces exerted on the pavement (e.g., by trucks, heavy machinery, airplanes), can be characterized by the following parameters:

- Tire loads
- Axle and tire configurations
- Repetition of loads
- Distribution of traffic across the pavement
- Vehicle speed

![H-1 during rush hour](https://pavementinteractive.org/wp-content/uploads/2008/07/Loadf1.jpg)

![Buses at Ala Moana](https://pavementinteractive.org/wp-content/uploads/2008/07/Loadf2.jpg)

*Figures 1 and 2.* H-1 during rush hour Buses at Ala Moana

Loads, along with the environment, damage pavement over time. The simplest pavement structural model asserts that each individual load inflicts a certain amount of unrecoverable damage. This damage is cumulative over the life of the pavement and when it reaches some maximum value the pavement is considered to have reached the end of its useful service life.

A wheel load bends the pavement layers beneath it. Directly under the load the upper part of the pavement is in compression and the lower part in tension; away from the load the pattern reverses. Damage accumulates through repeated cycles of loading and unloading, and cracking generally results from the tensile stresses. In [flexible pavements](https://pavementinteractive.org/glossary/flexible-pavement/) the asphalt and base layers resist both the compressive and tensile stresses; in [rigid pavements](https://pavementinteractive.org/glossary/rigid-pavement/) the concrete and any reinforcing steel carry the tension.

Therefore, pavement structural design requires a quantification of all expected loads a pavement will encounter over its design life. This quantification is usually done in one of two ways:

1. **Equivalent single axle loads (ESALs)**. This approach converts wheel loads of various magnitudes and repetitions ("mixed traffic") to an equivalent number of "standard" or "equivalent" loads.
2. **Load spectra**. This approach characterizes loads directly by number of axles, configuration and weight. It does not involve conversion to equivalent values. Structural design calculations using load spectra are generally more complex than those using ESALs.

Both approaches use the same type and quality of data but the load spectra approach has the potential to be more accurate in its load characterization.

## Tire Loads

Tire loads are the fundamental loads at the actual tire-pavement contact points. For most pavement analyses, it is assumed that the tire load is uniformly applied over a circular area. Also, it is generally assumed that tire inflation and contact pressures are the same (this is not exactly true, but adequate for approximations). The equation below relates the radius of tire contact to tire inflation pressure and the total tire load:

$$a = \sqrt{\frac{P}{p\pi}}$$

where:

- $$a$$ = radius of tire contact
- $$P$$ = total load on the tire
- $$p$$ = tire inflation pressure

States generally limit the allowable load per inch width of tire. Based on a slightly dated survey (Sharma, Hallin and Mahoney, 1983[^1]), this tire load limitation varies from a high of 140 N/mm (800 lbs/inch) to a low of 79 N/mm (450 lbs/inch).

![FHWA Class 9 five-axle tractor semi trailer (18 tires total). A typical tire load is 18.9 kN (4,250 lbs) with an inflation pressure of 689 kPa (100 psi.)](https://pavementinteractive.org/wp-content/uploads/2008/09/Semi_tires.jpg)

*Figure 3.* FHWA Class 9 five-axle tractor semi trailer (18 tires total). A typical tire load is 18.9 kN (4,250 lbs) with an inflation pressure of 689 kPa (100 psi.)

Tire width and inflation pressure also affect how a load reaches the pavement. Wider tires spread a load over a larger area, while higher inflation pressures concentrate it at the surface and lower pressures spread it out.

## Axle and Tire Configurations

While the tire contact pressure and area is of vital concern in pavement performance, the number of contact points per vehicle and their spacing is also critical. As tire loads get closer together their influence areas on the pavement begin to overlap, at which point the design characteristic of concern is no longer the single isolated tire load but rather the combined effect of all the interacting tire loads. Therefore, axle and tire arrangements are quite important.

Generally, the more contact points a load is spread over, the smaller each individual load and the less cumulative damage. Tandem axles, pairs of closely spaced axles, greatly reduce damage for the same load: an 18,000 lb load on a tandem axle produces roughly one tenth the ESALs of the same load on a single axle. Dual tires matter less than tandem axles, but for a given single axle load they reduce pavement stress by about 10 to 20 percent compared with single tires.

### Descriptions

Tire-axle combinations are typically described as (Figure 4):

- Single axle single tire(truck steering axles, etc.)
- Single axle dual tires
- Tandem axle single tires (Figure 5)
- Tandem axle dual tires

![Tire-axle combinations (from Mahoney, 1984).](https://pavementinteractive.org/wp-content/uploads/2008/09/Tire_axle.gif)

*Figure 4.* Tire-axle combinations (from Mahoney, 1984).

![Tandem drive axle on a tractor frame during manufacturing.](https://pavementinteractive.org/wp-content/uploads/2008/09/2_axle_configuration.jpg)

*Figure 5.* Tandem drive axle on a tractor frame during manufacturing.

### Typical Axle Load Limits

Federal and State laws establish maximum axle and gross vehicle weights to limit pavement damage. The range of weight limits in the U.S. vary a bit based on various Federal and State laws. Figure 6 shows the range of maximum limits for single axle, tandem axle and gross vehicle weight (GVW) established by the states and the FHWA.

![Range of allowable axle and truck weights in the U.S. (based on data from USDOT, 2000).](https://pavementinteractive.org/wp-content/uploads/2008/09/Load_limits.gif)

*Figure 6.* Range of allowable axle and truck weights in the U.S. (based on data from USDOT, 2000).

Although each state and the FHWA have established maximum axle-tire load combinations, there are other restrictions as well. One of the most common is the [FHWA bridge formula](https://pavementinteractive.org/reference-desk/design/structural-design/fhwa-bridge-formula/) (sometimes called the Federal Bridge Formula B).

## Repetition of Wheel Loads

Although it is not too difficult to determine the wheel and axle loads for an individual vehicle, it becomes quite complicated to determine the number and types of wheel/axle loads that a particular pavement will be subject to over its entire design life. Furthermore, it is not the wheel load but rather the damage to the pavement caused by the wheel load that is of primary concern.There are currently two basic methods for characterizing wheel load repetitions:

1. **Equivalent single axle load (ESAL)**. Based on [AASHO Road Test](https://pavementinteractive.org/reference-desk/design/structural-design/aasho-road-test/) results, the most common approach is to convert wheel loads of various magnitudes and repetitions ("mixed traffic") to an equivalent number of "standard" or "equivalent" loads. The most commonly used equivalent load in the U.S. is the 80 kN (18,000 lbs) [equivalent single axle load](https://pavementinteractive.org/glossary/equivalent-single-axle-load-esal/) (normally designated [ESAL](https://pavementinteractive.org/glossary/esal/)).
2. **Load spectra**.The 2002 G*uide for the Design of New and Rehabilitated Pavement Structures* (NCHRP 1-37A) essentially does away with the ESAL and determines loading directly from axle configurations and weights. This is a more precise characterization of traffic but relies on the same input data used to calculate ESALs. typical load spectrum input would be in the form of a table that shows the relative axle weight frequencies for each common axle combination (e.g. single axle, tandem axle, tridem axle, quad axle) over a given [time period](https://pavementinteractive.org/glossary/time-period/) (Figure 7). Often, load spectra data can be obtained from [weigh-in-motion stations](https://pavementinteractive.org/reference-desk/design/design-parameters/weigh-in-motion/).

![Example load spectra input screen from NCHRP 1-37A.](https://pavementinteractive.org/wp-content/uploads/2008/09/Aashto2002.gif)

*Figure 7.* Example load spectra input screen from NCHRP 1-37A.

Typically, designers must not only calculate ESALs or load spectra for various vehicles but also must forecast the expected number of ESALs or load spectra a pavement will encounter over its entire design life. This information then helps determine the structural design. Highway design in most states is based on the ESAL traffic input anticipated over a future 10 to 50 year period.

Load estimates matter in both directions. Underestimating loads leads to early failure and higher maintenance and rehabilitation costs, while overestimating them produces an over-designed pavement with unnecessary initial cost.

## Traffic Distribution

Along with load type and repetitions, the load distributions across a particular pavement must be estimated. For instance, on a 6-lane interstate highway (3 lanes in each direction) the total number of loads is probably not distributed exactly equally in both directions. Often one direction carries more loads than the other. Furthermore, within that one direction, not all lanes carry the same loading. Typically, the outer most lane carries the most trucks and therefore is subjected to the heaviest loading. Therefore, pavement structural design should account for these types of unequal load distribution. Typically, this is accounted for by selecting a "design lane" for a particular pavement. The loads expected in the design lane are either (1) directly counted or (2) calculated from the cumulative two-direction loads by applying factors for directional distribution and lane distribution. The 1993 AASHTO *Guide* offers the following basic equation:

$$w_{18} = D_D \times D_L \times \hat{w}_{18}$$

where:

- $$w_{18}$$ = traffic (or loads) in the design lane
- $$D_D$$ = a directional distribution factor, expressed as a ratio, that accounts for the distribution of loads by direction (e.g., east-west, north-south). For instance, one direction may carry a majority of the heavy truck loads and thus it would either be designed differently or, at a minimum, it would control the structural design. Generally taken as 0.5 (50%) for most roadways unless more detailed information is known.
- $$D_L$$ = a lane distribution factor, expressed as a ratio, that accounts for the distribution of loads when two or more lanes are available in one direction. For instance, on most interstate routes, the outside lane carries a majority of the heavy truck traffic. The table below gives typical values.
- $$\hat{w}_{18}$$ = the cumulative two-directional loads predicted for a specific section of highway during the design period.

**Table 1.** Percent of loads in the design lane, by number of lanes in each direction

| Number of Lanes in Each Direction | Percent of Loads in Design Lane |
| --- | --- |
| 1 | 100 |
| 2 | 80–100 |
| 3 | 60–80 |
| 4 | 50–75 |

## Vehicle Speed

Although current design practices do not necessarily account for vehicle speed, it does influence pavement loading. In general, slower speeds and stop conditions allow a particular load to be applied to a given pavement area for a longer period of time resulting in greater damage. For HMA pavements this behavior is sometimes evident at bus stops (where heavy buses stop and sit while loading/unloading passengers) and intersection approaches (where traffic stops and waits to pass through the intersection) when [mix design](https://pavementinteractive.org/reference-desk/design/mix-design/) or [structural design](https://pavementinteractive.org/reference-desk/design/structural-design/) have been inadequate. In HMA pavement design, [Superpave](https://pavementinteractive.org/reference-desk/design/mix-design/superpave-gradation-requirements/) accounts for vehicle speed indirectly by applying a design pavement temperature adjustment for slow-moving or stopped vehicles.

## [The Equivalent Single Axle Load](https://pavementinteractive.org/reference-desk/design/design-parameters/equivalent-single-axle-load/)

Although it is not too difficult to determine a wheel or an axle load for an individual vehicle, it becomes quite complicated to determine the number and types of wheel/axle loads that a particular pavement will be subject to over its design life. Furthermore, it is not the wheel load but rather the damage to the pavement caused by the wheel load that is of primary concern. The most common historical approach is to convert damage from wheel loads of various magnitudes and repetitions ("mixed traffic") to damage from an equivalent number of "standard" or "equivalent" loads. The most commonly used equivalent load in the U.S. is the 18,000 lb (80 kN) equivalent single axle load (normally designated ESAL). At the time of its development (early 1960s at the [AASHO Road Test](https://pavementinteractive.org/reference-desk/design/structural-design/aasho-road-test/)) it was much easier to use a single number to represent all traffic loading in the somewhat complicated empirical equations used for predicting pavement life.

### Load Equivalency

Using the ESAL method, damage from all loads (including multi-axle loads) are converted to damage from an equivalent number of 18,000 lb. single axle loads, which is then used for design. A "load equivalency factor" represents the equivalent number of ESALs for the given weight-axle combination. The equation used to determine load equivalency can be quite complicated. As a rule-of-thumb, the load equivalency of a particular load (and also the pavement damage imparted by a particular load) is roughly related to the load by a power of four (for reasonably strong pavement surfaces). For example, a 36,000 lb. single axle load will cause about 16 times the damage as an 18,000 lb. single axle load.

Table 1 shows some typical load equivalencies (note that spreading a load out over two closely spaced axles reduces the number of ESALs). Figure 8, using some approximations, shows some general vehicle load equivalencies - note that buses tend

**Table 2.**

| Load | Number of ESALs |
| --- | --- |
| 18,000 lb. single axle | 1.000 |
| 2,000 lb. single axle | 0.0003 |
| 30,000 lb. single axle | 7.9 |
| 18,000 lb. tandem axle | 0.109 |
| 40,000 lb. tandem axle | 2.06 |

![Some typical Load Equivalency Factors](https://pavementinteractive.org/wp-content/uploads/2008/07/LEQs.gif)

*Figure 8.* Some typical Load Equivalency Factors

Load equivalency factors depend on pavement type (flexible or rigid) and on the strength of the pavement structure. Because of the fourth-power relationship, a modestly loaded truck does as much damage as thousands of passenger cars, and loads from motorcycles, passenger cars, pickup trucks and vans are generally treated as negligible in structural design. The ESAL approach dates from the [AASHO Road Test](https://pavementinteractive.org/reference-desk/design/structural-design/aasho-road-test/) of the early 1960s and is still widely used.

- Traffic Index (TI). The traffic index is associated with the California method of pavement structural design. Essentially, it has evolved in to a way of expressing ESALs as a single number or index (see Figure 9).

![Traffic Index vs. ESALs](https://pavementinteractive.org/wp-content/uploads/2008/07/TrafficIndexvsEsals.gif)

*Figure 9.* Traffic Index vs. ESALs

## Load Spectra

The 2002 *Guide for the Design of New and Rehabilitated Pavement Structures* (NCHRP 1-37A) has gone away from the [ESAL approach](https://pavementinteractive.org/reference-desk/design/design-parameters/equivalent-single-axle-load/) and adopted a load spectra approach. In essence, the load spectra approach uses the same traffic data that the ESAL approach uses only it does not convert the loads into ESALs – it maintains the data by axle configuration and weight. This information can then be used with a series of mechanistic-empirical equations to develop a pavement structural design. Some key advantages of the load spectra approach are:

1. It is compatible with the FHWA's *Traffic Monitoring Guide* (TMG) and thus many agencies are already collecting the appropriate data.
2. It offers a hierarchical approach to traffic data input depending upon the users needs and resources. There are three levels of potential input:

   - *Level 1 Inputs* – Use of volume/classification and axle load spectra data directly related to the project.
   - *Level 2 Inputs* – Use of regional axle load spectra data and project-related volume/classification data**.**
   - *Level 3 Inputs* – Use of regional or default classification and axle load spectra data.

3. It already includes information on traffic distribution including directional, lane and temporal distribution (if needed) as well as traffic growth rates.

## Sources

[^1]: Hallin and Mahoney (1983). Evaluation of Present Legislation and Regulations on Tire Sizes, Configurations and Load Limits. Research Report WA-RD 59.1, Washington State Department of Transportation. Olympia, WA.