# Tie Bar Placement

Tie bars are typically placed after PCC placement either by hand or using a tie bar inserter attachment (slipform paving only).

- Canonical URL: https://pavementinteractive.org/reference-desk/construction/placement/tie-bar-placement/
- Last updated: 2026-11-01
- Review: reviewed by licensed professional engineers on the previous Pavement Interactive site, where reviewers were not recorded by name

[Tie bars](https://pavementinteractive.org/reference-desk/pavement-types-and-history/pavement-types/tie-bars/) are typically placed after PCC placement either by hand or using a tie bar inserter attachment ([slipform paving](https://pavementinteractive.org/reference-desk/construction/placement/slipform-paving/) only). When one lane at a time is paved, tie bars are inserted at mid-slab depth and bent back until the adjacent lane is ready to be paved (see Figure 1). On slipform pavers, tie bars are inserted on slab edges that will become longitudinal joints (see Figure 2 and 3) and, if two lanes at once are being paved, pushed into a mid-slab area (similar to [dowel bar](https://pavementinteractive.org/glossary/dowel-bar/) insertion) that will later be cut as a longitudinal joint (see Figure 4 and 5). Like dowel bars, tie bars should be protected from corrosion.

![Bent tie bars.](https://pavementinteractive.org/wp-content/uploads/2010/04/Tie_bar_inserter2.jpg)

![Side tie bar inserter.](https://pavementinteractive.org/wp-content/uploads/2010/04/Tie_bar_inserter3.jpg)

*Figures 1 and 2.* Bent tie bars. Side tie bar inserter.

![Tie bar insertion equipment for side tie bars.](https://pavementinteractive.org/wp-content/uploads/2010/04/Tie_bar4.jpg)

*Figure 3.* Tie bar insertion equipment for side tie bars.

![Inserter for mid-slab tie bars (the area in which the tie bars are inserted will later be cut as a longitudinal joint).](https://pavementinteractive.org/wp-content/uploads/2010/04/Tie_bar2.jpg)

![Tie bar insertion cartridge protruding upward from the center of a slipform paver.](https://pavementinteractive.org/wp-content/uploads/2010/04/Tie_bar_inserter1.jpg)

*Figures 4 and 5.* Inserter for mid-slab tie bars (the area in which the tie bars are inserted will later be cut as a longitudinal joint). Tie bar insertion cartridge protruding upward from the center of a slipform paver.