# Paving Equipment

A stabilizer/reclaimer is a vehicle with a dual purpose.

- Canonical URL: https://pavementinteractive.org/reference-desk/construction/placement/paving-equipment/
- Last updated: 2018-09-21
- Review: reviewed by licensed professional engineers on the previous Pavement Interactive site, where reviewers were not recorded by name

## Stabilizers/Reclaimers

A stabilizer/reclaimer is a vehicle with a dual purpose. These machines have a large rotor blade which may be used to cut and pulverize damaged or old [pavement](https://pavementinteractive.org/reference-desk/pavement-types-and-history/pavement-types/hma-pavement/), but which also may be used to mix lime, fly ash, or cement into the [subbase](https://pavementinteractive.org/reference-desk/pavement-types-and-history/pavement-types/hma-pavement/) in order to stabilize poor soils.

## Milling Machines

A top layer is milled off the existing pavement to provide a relatively smooth surface on which to pave. Milling is also commonly used to remove a distressed [surface layer](https://pavementinteractive.org/glossary/surface-layer/) from an existing pavement. Milling machines are the primary method for removing old HMA pavement surface material prior to overlay. They can be fitted with automatic grade control to restore both longitudinal and transverse grade and can remove most existing pavement distortions. Milling also produces a rough, grooved surface, which will increase the existing pavement’s surface area when compared to an ungrooved surface. The surface area increase is dependent on the type, number, condition and spacing of cutting drum teeth but is typically in the range of 20 to 30 percent, which requires a corresponding increase in tack coat (20 to 30 percent more) when compared to an unmilled surface. Milling is advantageous because it:

- Provides RAP for recycling operations.
- Efficiently removes deteriorated pavement that is unsuitable for retention in the overlaid pavement.
- Provides a highly skid resistant surface suitable for temporary use by traffic until the final surface can be placed.
- Allows curb and gutter lines to be maintained or re established before HMA overlays.
- Provides an efficient removal technique for material near overhead structures in order to maintain clearances for bridge structures, traffic signals and overhead utilities.

![Side view of milling machine.](https://pavementinteractive.org/wp-content/uploads/2008/08/Millingmachine1.jpg)

![Cutting tips on rotary drum.](https://pavementinteractive.org/wp-content/uploads/2008/08/Millingmachine2.jpg)

*Figures 1 and 2.* Side view of milling machine. Cutting tips on rotary drum.

## Graders

Graders may be used in place of milling machines if the base course is dirt or gravel. They are vehicles with large blades that create a wide flat surface for [asphalt](https://pavementinteractive.org/reference-desk/materials/asphalt/introduction/) to be placed on.

![A grader preparing the subgrade on a project on SR 528 in Marysville, WA.](https://pavementinteractive.org/wp-content/uploads/2008/08/Graderpic.jpg)

*Figure 3.* A grader preparing the subgrade on a project on SR 528 in Marysville, WA.

## Sweepers

Sweepers clean the surface of the road after it has been milled or graded. This is necessary because excessive dust and debris on the ground can prevent proper bonding between the asphalt and the base course. Large pieces of debris can also cause non-uniform compaction of the asphalt.

![Sweeping machine.](https://pavementinteractive.org/wp-content/uploads/2008/08/Sweeper.jpg)

*Figure 4.* Sweeping machine.

## Batch Plant

Batch plants, which produce HMA in individual batches, are the older of the two types of HMA production facilities; it was not until the 1970s that drum plants became a popular HMA production option. Typical batch quantities range from 1.5 to 5 tons of HMA and each batch can take 15 - 45 seconds to make.

![Batch plant](https://pavementinteractive.org/wp-content/uploads/2008/08/Batchplant.jpg)

*Figure 5.* Batch plant

## Drum Plant

Drum plants, which produce HMA in a continuous manner, generally offer higher production rates than batch plants for comparable cost. Typical production rates for drum plants vary between about 100 tons/hr up to over 900 tons/hr depending upon drum design.

![A continuous or drum plant.](https://pavementinteractive.org/wp-content/uploads/2008/08/Drumplant.jpg)

*Figure 6.* A continuous or drum plant.

## Dump Trucks

Dump trucks move the hot asphalt from the plant to the jobsite. There are many kinds of dump trucks:

- End dump: unload their payload by raising the front end and letting the payload slide down the bottom of the bed and out the back through a tailgate. They are the most popular transport vehicle type because they are plentiful, maneuverable and versatile.
- Bottom or belly dump: Bottom dump trucks unload their payload by opening gates on the bottom of the bed. Internal bed walls are sloped to direct the entire payload out through the opened gates. Discharge rates can be controlled by the degree of gate opening and the discharge is usually placed in an elongated pile, called a windrow, in front of the paver by driving the truck forward during discharge. Windrows require a special MTV (material transfer vehicle) to feed the HMA into the paver.
- Live bottom or flo-boy: Live bottom dump trucks have a conveyor system at the bottom of their bed to unload their payload. HMA is discharged out the back of the bed without raising the bed. Live bottom trucks are more expensive to use and maintain because of the conveyor system but they also can reduce segregation problems and can eliminate some detrimental types of truck bed – paver contact (because the bed is not raised during discharge).

![End dump truck placing WMA into a skip.](https://pavementinteractive.org/wp-content/uploads/2008/08/CelesteEndDumpPhoto2.jpg)

*Figure 7.* End dump truck placing WMA into a skip.

## Material Transfer Vehicles

Material transfer vehicles (MTVs) are used to assist the paver in accepting HMA. Most pavers are equipped to receive HMA directly from end dump or live bottom trucks, however in certain situations it can be necessary or advantageous to use an MTV. Paving using bottom dump trucks and windrows requires a windrow elevator MTV, while other MTVs are used to provide additional surge volume, which is advantageous because it allows the paver to operate continuously without stopping, minimizes truck waiting time at the paving site and may minimize aggregate segregation and temperature differentials.

![Material transfer vehicle, or shuttle buggy.](https://pavementinteractive.org/wp-content/uploads/2008/08/MTV.jpg)

*Figure 8.* Material transfer vehicle, or shuttle buggy.

## Asphalt Pavers

The [asphalt paver](https://pavementinteractive.org/reference-desk/construction/placement/asphalt-paver/) is a self-propelled formless laydown machine with a floating screed. HMA is loaded in the front, carried to the rear by a set of flight feeders (conveyor belts), spread out by a set of augers, then leveled and compacted by a screed. This set of functions can be divided into two main systems:

- Tractor: The tractor contains the material feed system, which accepts the HMA at the front of the paver, moves it to the rear and spreads it out to the desired width in preparation for screed leveling and compaction.
- Screed: The most critical feature of the paver is the self-leveling screed unit, which determines the profile of the HMA being placed (Roberts et al., 1996[^1]). The screed takes the head of HMA from the material delivery system, strikes it off at the correct thickness and provides initial mat compaction. Figure 5 shows screed components and the six basic forces that act upon the screed to determine its height and, thus, pavement thickness.

The screed helps control the amount of material extruded onto the base course, flattening the asphalt on the ground. It also assists in offering a level surface for compaction regardless of the condition of the base course. However, the base course needs to be reasonably level in order to prevent future cracking.

![A typical asphalt paving machine.](https://pavementinteractive.org/wp-content/uploads/2008/08/PaverAstec.jpg)

*Figure 9.* A typical asphalt paving machine.

## Compactors/Rollers

There are three basic pieces of equipment available for HMA compaction: (1) the paver screed, (2) the steel wheeled roller and (3) the pneumatic tire roller. Each piece of equipment compacts the HMA by two principal means:

1. By applying its weight to the HMA surface and compressing the material underneath the ground contact area. Since this compression will be greater for longer periods of contact, lower equipment speeds will produce more compression. Obviously, higher equipment weight will also increase compression.
2. By creating a shear stress between the compressed material underneath the ground contact area and the adjacent uncompressed material. When combined with equipment speed, this produces a shear rate. Lowering equipment speed can decrease the shear rate, which increases the shearing stress. Higher shearing stresses are more capable of rearranging aggregate into more dense configurations.

These two means are of compacting HMA are often referred to collectively as “[compactive effort](https://pavementinteractive.org/glossary/compactive-effort/)”.

### Paver Screed

Approximately 75 to 85 percent of [theoretical maximum density](https://pavementinteractive.org/reference-desk/design/mix-design/hma-weight-volume-terms-and-relationships/), or [Rice density](https://pavementinteractive.org/glossary/rice-density/), will be obtained when the mix passes out from under the screed.

### Steel Wheel Rollers

Steel wheel rollers are self-propelled compaction devices that use steel drums to compress the underlying HMA. They can have one, two or even three drums, although tandem (2 drum) rollers are most often used. The drums can be either static or vibratory and usually range from 35 to 85 inches in width and 20 to 60 inches in diameter. Roller weight is typically between 1 and 20 tons.

Some steel wheel rollers are equipped with vibratory drums. Drum vibration adds a dynamic load to the static roller weight to create a greater total compactive effort. Drum vibration also reduces friction and [aggregate interlock](https://pavementinteractive.org/glossary/aggregate-interlock/) during compaction, which allows aggregate particles to move into final positions that produce greater friction and interlock than could be achieved without vibration. As a general rule-of-thumb, a combination of speed and frequency that results in 10 - 12 impacts per foot is good. At 3000 vibrations/minute this results in a speed of 2.8 - 3.4 mph.

![A steel wheel roller](https://pavementinteractive.org/wp-content/uploads/2008/08/Roller.jpg)

*Figure 10.* A steel wheel roller

### Pneumatic Tire Rollers

Pneumatic tire rollers are self-propelled compaction devices that uses pneumatic tires to compact the underlying HMA. Pneumatic tire rollers employ a set of smooth (no tread) tires on each axle; typically four or five on one axle and five or six on the other. The tires on the front axle are aligned with the gaps between tires on the rear axel to give complete and uniform compaction coverage over the width of the roller. Compactive effort is controlled by varying tire pressure, which is typically set between 60 and 120 psi. In addition to a static compressive force, pneumatic tire rollers also develop a kneading action between the tires that tends to realign aggregate within the HMA. Because [asphalt binder](https://pavementinteractive.org/glossary/asphalt-binder/) tends to stick more to cold tires than hot tires, the tire area is often insulated with rubber matting or plywood to maintain the tires near mat temperature while rolling.

![A pneumatic tire roller compacting chip seal.](https://pavementinteractive.org/wp-content/uploads/2008/08/Pneumatictireroller.jpg)

*Figure 11.* A pneumatic tire roller compacting chip seal.

## References

- *Washington Asphalt Pavement Guide*, Washington Asphalt Pavement Association, Inc., 2002

## Sources